04-24-2008, 09:39 PM
it depends...
If you have a finished helmet with that thickness, probably it's good. To get that thickness in a finished helmet, you have begin with a thicker iron plate, and hammering and forming it you get that 1 mm.
It's not the same 1 mm of a rolled plate that 1 mm of hammer beaten plate (it's a lot stronger). And original helmets commonly are very thin walled.
If you have a finished helmet with that thickness, probably it's good. To get that thickness in a finished helmet, you have begin with a thicker iron plate, and hammering and forming it you get that 1 mm.
It's not the same 1 mm of a rolled plate that 1 mm of hammer beaten plate (it's a lot stronger). And original helmets commonly are very thin walled.